Bio:
Jeffrey C. Suhling received his Ph.D. degree in Engineering Mechanics from the University of Wisconsin in 1985. He then joined the faculty of the Department of Mechanical Engineering at Auburn University, and currently holds the rank of Quina Distinguished Professor. He served as the Center Director for the NSF Center for Advanced Vehicle Electronics (CAVE) from 2002-2008, and as ME Department Chair from 2008-2025. His research concentrates on the mechanics, reliability, and materials science of electronic packaging and semiconductors; with emphasis on material characterization and constitutive modeling, and reliability testing and modeling, and stress sensors and test chips. Dr. Suhling has co-authored over 600 technical publications on electronics packaging, with over 15,000 citations and an H-Index of 63 on Google Scholar. He has advised over 100 graduate students at Auburn University including over 40 PhD students working in the electronics industry and academia. He is a Fellow of ASME, Senior Member of IEEE, and member of SMTA and IMAPS. Dr. Suhling has been a member of the IEEE Electronics Packaging Society for the past 35 years, and is serving as Society President for a two-year term in 2026-2027. He received the EPS William Chen Distinguished Service Award in 2024.
Abstract:
Lead-free solder interconnections of several length scales are typically utilized in advanced packaging architectures employed for heterogenous integration such as System in Package (SIP), 2.3D, 2.5D, 3D, etc. These include micro bumps between the silicon die and interposer, flip chip (C4) joints between interposer and package substrate, and larger BGA joints between package substrate and PCB. The size differences between these interconnection levels typically spans 2-3 orders of magnitude. In applications such as AI data centers, these solder joints can be exposed to sustained high temperature operation at temperatures exceeding 100 oC, as well as potential thermal cycling to higher extremes. This talk discusses several reliability challenges that are present in the various levels of lead-free solder interconnections in advanced packaging. In particular, the effects of solder aging during high temperature exposure, of solder damage accumulation during temperature cycling, and of solder joint orientation variations in micro bumps will be discussed.
All levels of solder interconnections in advanced packaging are affected by aging effects and damage accumulation, where their mechanical behavior and failure properties degrade with time when exposed to isothermal or variable temperature environments. Such degradations are caused by the unstable microstructures present at relatively low temperatures and by microcrack growth, and they can lead to a significant reduction in the reliability of electronic products with time. An overview of solder behavior changes due to aging and damage accumulation will be presented including imagery of microstructural evolution and microcrack growth in solder joints, and measurements of the resulting stress-strain, material property, and creep rate degradations. The effects of crystal orientation variations are only present in solder micro joints. Since they are so small, there is typically only one anisotropic single crystal tin grain in each joint that is reinforced with Sn-Ag or Sn-Cu intermetallic particles. This results in each micro joint having unique mechanical behavior. The implications of these variations are demonstrated through mechanical testing using nanoindentation, as well as anisotropic crystal plasticity finite element simulations using custom material subroutines.