S14 【S14】Advanced Bonding Technologies
Oct. 20, 2026 13:00 PM - 15:00 PM
Room: 702, 7F, TaiNEX 2
Session chair: Jenn-Ming Song, National Chung Hsing University / Yeong-Jyh Lin, National Sun Yat-sen University
Smoothing of Bonding Interfaces via Thin-Film Transfer Technology and Applications to Low-Temperature Bonding
發表編號:S14-2時間:13:00 - 13:30 |

Invited Speaker
Speaker: Eiji Higurashi, Professor, Tohoku University
Bio:
Eiji Higurashi received the M.E. and Ph.D. degrees from Tohoku University in 1991 and 1999, respectively. From 1991 to 2003, he worked for the Nippon Telegraph and Telephone Corporation (NTT). From 2003 to 2017, he was an Associate Professor at The University of Tokyo. From 2017 to 2022, he was a team leader or group leader at The National Institute of Advanced Industrial Science and Technology (AIST). Since 2022, he has been a Professor at Tohoku University, Japan. He serves as the president of The Japan Institute of Electronics Packaging (JIEP) and as a member of Board of Governors (BoG) of IEEE EPS.
Abstract:
Surface-activated bonding (SAB) is a method of bonding activated solid surfaces using adhesive forces between surface atoms. It requires extremely smooth bonding surfaces (root-mean-square roughness: 1 nm or less), and there is a major issue of difficulty in bonding when ultra-precision polishing processes, such as chemical mechanical polishing (CMP), cannot be applied. In response, we developed a smoothing method using additive processing by combining template stripping and surface-activated bonding. We demonstrated the smoothing of plated Au surfaces for direct Au bonding at room temperature.
|
|
Quantitative Nano-Topography Analysis of Wafer Edge Roll-Off for High-Volume Wafer-to-Wafer Bonding Applications
發表編號:S14-3時間:13:30 - 13:45 |
![]()
Paper ID:AS0146 Speaker: Joonho You Author List: Joonho You, Jaeyoung Jang, Myungsoo Choi
Bio: Biography Joonho You is the Chief Executive Officer (CEO) of Nexensor Inc. He studied optical metrology at Korea Advanced Institute of Science and Technology (KAIST) and has more than 20 years of experience in the research, development, and commercialization of optical metrology technologies.
His research interests include interferometric metrology, thin-film measurement technologies, shape measurement techniques based on structured light projection methods such as deflectometry and Moiré techniques, and fiber-optic sensing technologies for thickness measurement.
He currently serves as an Director of the Inspection and Metrology Division of the Korean Microelectronics and Packaging Society (KMEPS) and Optical Society of Korea (OSK).
Abstract: As semiconductor packaging technologies continue to evolve toward higher integration densities, wafer-to-wafer (W2W) bonding has emerged as a key enabling process for advanced three-dimensional (3D) integration, heterogeneous integration, and hybrid bonding applications. The success of W2W bonding strongly depends on the surface topography and edge geometry of the wafers being bonded. Among various geometric parameters, wafer edge roll-off (ERO), defined as the gradual deviation of wafer surface height near the wafer edge, has become an increasingly critical factor affecting bonding yield, overlay accuracy, wafer handling stability, and post-bonding reliability. Excessive edge roll-off may induce localized gaps, non-uniform bonding pressure distribution, void formation, and edge-related defects, ultimately reducing manufacturing yield and device performance. Consequently, accurate characterization of ERO at nanometer-scale resolution has become an essential metrology requirement for high-volume semiconductor manufacturing.
Various metrology techniques have been investigated for ERO measurement. Atomic Force Microscopy (AFM) is widely recognized for its exceptional vertical resolution at the nanometer and sub-nanometer scale. AFM enables detailed characterization of local surface morphology and provides highly accurate topographic information. However, its practical application to ERO inspection in production environments is limited by its relatively small field of view, slow scanning speed, and difficulty in measuring long edge profiles over several millimeters. As semiconductor manufacturing increasingly demands full-wafer and high-throughput inspection capabilities, AFM is primarily utilized for reference measurements and localized verification rather than inline process monitoring.
Optical triangulation techniques represent another widely adopted approach for measuring wafer edge geometry. These methods offer non-contact operation, relatively simple system architectures, and fast acquisition speeds. Optical triangulation can efficiently measure large-scale geometric profiles and is often used for wafer edge inspection and dimensional metrology. Nevertheless, its measurement accuracy is fundamentally constrained by spot size, sensor resolution, and triangulation geometry. Furthermore, measurement uncertainty tends to increase when inspecting highly reflective semiconductor surfaces or when nanometer-level height precision is required. These limitations restrict the applicability of optical triangulation for advanced hybrid bonding processes where extremely tight topography specifications must be satisfied.
Interferometric metrology has emerged as a promising solution for overcoming the limitations of existing measurement techniques. By exploiting optical phase information, interferometric systems provide nanometer-scale vertical resolution while maintaining a relatively large measurement field and high acquisition efficiency. Various interferometric approaches, including phase-shifting interferometry (PSI), white-light interferometry (WLI), and coherence scanning interferometry (CSI), have demonstrated excellent capability in measuring ultra-flat semiconductor surfaces. However, the measurement of wafer edge roll-off presents unique challenges due to steep local slopes, large measurement ranges, and the requirement for high-speed operation compatible with mass-production environments.
In this study, a high-precision and high-speed interferometric metrology system was developed specifically for quantitative ERO characterization in wafer-to-wafer bonding applications. The proposed system combines advanced interferometric measurement principles with optimized optical design and dedicated signal processing algorithms to achieve accurate edge profile reconstruction over extended measurement regions. Unlike conventional interferometric systems that are often optimized for central wafer inspection, the developed architecture was designed to maintain measurement fidelity in the wafer edge region where topographic gradients become increasingly significant.
The developed methodology enables nanometer-scale vertical measurement precision while covering the entire ERO region within a single measurement sequence. Through optimized acquisition strategies and high-speed image processing, the system significantly reduces measurement time compared with traditional scanning-based methods. Experimental evaluations were performed using semiconductor wafers representative of advanced packaging processes. The measurement results demonstrated excellent repeatability, reproducibility, and correlation with reference metrology methods. The proposed interferometric approach successfully captured subtle edge profile variations that are difficult to resolve using conventional optical triangulation systems while achieving substantially higher throughput than AFM-based measurements.
Furthermore, the obtained ERO profiles provided valuable quantitative information for process optimization and quality control in wafer bonding production lines. The ability to rapidly characterize edge topography enables early detection of process-induced variations, supports wafer quality classification, and contributes to improved bonding yield prediction. The measurement data can also serve as an important input for process modeling and predictive manufacturing frameworks aimed at reducing defect formation during bonding operations.
In conclusion, accurate ERO characterization is becoming increasingly important as wafer-to-wafer bonding technologies advance toward tighter process tolerances and higher manufacturing volumes. While AFM and optical triangulation each offer unique advantages, their limitations in throughput, measurement range, or precision restrict their effectiveness for high-volume production environments. The interferometric metrology system presented in this work demonstrates that high-speed and high-precision ERO measurement can be simultaneously achieved through optimized interferometric design. The proposed approach provides nanometer-scale measurement capability, large-area coverage, and production-compatible throughput, making it a highly promising solution for next-generation semiconductor bonding processes. The developed technology is expected to contribute significantly to process control, yield enhancement, and reliability improvement in advanced semiconductor manufacturing.
|
|
Investigation of Fine-Pitch Gold-to-Gold Direct Bonding of Patterned Micro-Pads for High-Resolution Micro-Displays and Advanced Heterogeneous Packaging
發表編號:S14-4時間:13:45 - 14:00 |
![]()
Paper ID:TW0073 Speaker: Jui Lin Lu Author List: Po Chih Chang, Jui Lin Lu, Yi-Chen Chung, Yu-Hsiang Chang, Chu-Yin Hung, Pei-Hsuan Yeh, Wei-Hung Kuo, Sin-Jhu Wun, Pei-Ting Chou, Weileun Fang, Chih Chen
Bio: Jui Lin Lu is currently a Master's student in the Department of Institute of Pioneer Semiconductor Innovation at National Yang Ming Chiao Tung University. His research interests mainly focus on advanced packaging and semiconductor materials.
Abstract: With the rapid advancement of next-generation augmented reality (AR) near-to-eye displays and high-performance computing (HPC) hardware, the technical demand for high-density, high-bandwidth, and low-latency vertical interconnects has significantly escalated across the semiconductor industry. To achieve sub-10 micrometer pixel pitches in monolithic Micro-LED displays, conventional solder-based bump bonding schemes encounter severe physical and manufacturing limits, such as solder bridging, brittle intermetallic compound (IMC) formation, and high thermal budgets during reflow. Consequently, gold-to-gold (Au-Au) direct bonding at low temperatures has emerged as a highly compelling alternative, offering exceptional electrical conductivity, superior thermal dissipation, and excellent chemical stability. In this study, patterned Au pads with four distinct micro-scale dimensions 14, 8, 4, and 2 micrometers are successfully designed, fabricated, and characterized, specifically tailored for ultra-fine-pitch optoelectronic and heterogeneous integration. Unlike conventional sputtered metal schemes, the fabricated interconnect structure comprises a total metallization thickness of 1.0 micrometer, featuring a 600 nm-thick functional Au layer fabricated by a precise lift-off process deposited over a 400 nm-thick adhesion and diffusion barrier underlayer. Atomic force microscopy (AFM) characterization of the micro-pads reveals a highly uniform surface morphology with an average surface roughness (Ra) of 4.22 nm across all pad geometries, representing a typical micro-scale topography of lift-off metallization. This paper systematically evaluates the surface topography, structural integrity, and scaling effects of these micro-pads. Based on the measured surface roughness of 4.22 nm, a comprehensive analytical assessment of the thermo-mechanical requirements for successful solid-state diffusion bonding is conducted. While atomically flat surfaces (Ra < 1.0 nm) are traditionally desired for pressure less room-temperature surface-activated bonding (SAB), the obtained roughness of 4.22 nm indicates that a controlled thermo-compression process is necessary to facilitate localized plastic deformation at the micro-asperities. The 600 nm Au film thickness provides an optimal metallurgical balance, offering sufficient ductile volume to absorb the 4.22 nm surface asperities while successfully mitigating the risk of lateral metal squeeze-out and electrical shorting at the ultra-fine 2 micrometer pad pitch. Theoretical modeling of the bonding interface indicates that a high-quality, void-free joint can be accomplished at temperatures below 300 degrees Celsius under optimized bonding pressures, which effectively prevents thermal degradation of active optoelectronic devices. The scaling behavior of the 2, 4, 8, and 14 micrometer pads is thoroughly analyzed to delineate the critical relationship between pad area, contact compliance, and resulting shear strength. This study provides a solid foundation for optimizing the bond parameters of sub-five-micrometer gold pads, establishing a high-yield process flow for cost-effective micro-system manufacturing under strict thermal budget limits. These research findings demonstrate that the fabricated micro-pads are highly viable for enabling robust, ultra-fine-pitch vertical interconnects, thereby successfully bridging the technical gap between high-yield advanced packaging and next-generation high-resolution AR micro-display integration.
|
|
Sequential VUV-Citric Acid Valence-State Engineering of Cu Bump Surfaces for Low-Temperature Cu-Cu Hybrid Bonding in Advanced Packaging
發表編號:S14-5時間:14:00 - 14:15 |
![]()
Paper ID:AS0162 Speaker: Lokesh Selvi Palanisamy Author List: Lokesh Selvi Palanisamy, Yu-Hao Lo, Heng-Ching Mie, Jun Mizuno
Bio: Lokesh Selvi Palanisamy is a Ph.D. student at the Academy of Innovative Semiconductor and Sustainable Manufacturing, National Cheng Kung University, Taiwan. His research focuses on advanced heterogeneous integration, including surface activation studies, Organic dielectrics, EIC–PIC co-packaged optics, SiC interposers, and Ga₂O₃–SiC thermal integration. His work also includes microfluidic and vapor-chamber thermal management for high-power semiconductor packages. Before joining NCKU, he conducted research on high-energy propellants and energetic-material characterization at the Defence Institute of Advanced Technology - DRDO, India.
Abstract: INTRODUCTION Fine-pitch Cu–Cu hybrid bonding is a key interconnection technology for chiplet integration, high-bandwidth memory, and co-packaged optics, enabling solderless interconnection with reduced pitch, lower parasitic loss, and higher vertical integration density. However, Cu bump surfaces are highly vulnerable to organic contamination and native oxidation during the queue time between surface activation, alignment, and bonding. Native Cu oxide generally forms a multilayer structure, with Cu2O-rich–(a p-type semiconductor) Cu1+ near the metallic Cu base and CuO/Cu(OH)2 -rich Cu2+ species at the outer surface. The Cu2+-rich layer acts as a resistive, defect-rich barrier that suppresses intimate Cu–Cu contact and increases contact-resistance fluctuation[1]. Therefore, this work implements sequential 172 nm VUV irradiation and citric-acid treatment on Cu bump chips as a low-temperature, mechanism-driven Cu valence-state control route for organic removal, Cu2+ suppression, citrate passivation, and improved low temperature Cu–Cu bonding. CONCEPT & METHOD The proposed process separates dry VUV activation from wet chemical passivation. The 172 nm VUV irradiation decomposes adventitious carbon and oxygen-containing residues through C–C, C–H, and C–O bond scission[2], while citric acid selectively chelates Cu oxide/hydroxide species, especially Cu2+-rich CuO/Cu(OH) 2, forming a temporary Cu–citrate/carboxylate termination[3]. This ultrathin passivation layer is designed to suppress non-uniform re-oxidation during queue time while remaining transformable or removable during thermal compression bonding. CMP-planarized Cu bump chips and blanket Cu reference samples were processed using VUV-only, citric-acid-only, and sequential routes. Surface chemistry was evaluated by XPS C 1s, O 1s, Cu 2p, and Cu LMM Auger spectra to resolve Cu0, Cu1+, and Cu2+ states[1]. ATR-FTIR verified citrate/carboxylate coordination, while AFM/contact-angle measurements evaluated morphology and activation. Treated Cu bump chips were bonded below 250 °C using immediate and delayed splits to evaluate queue-time stability and low-temperature bonding compatibility. BONDING VALIDATION For packaging validation, the VUV/citric-acid process is implemented on Cu bump test chips and evaluated against untreated, VUV-only, and citric-acid-only controls. C-SAM/SAT inspection is used to quantify bonded area and interfacial voiding; die shear evaluates mechanical strength; cross-sectional SEM/EDS examine Cu-Cu interfacial continuity and residual C/O; and Kelvin/daisy-chain structures verify electrical continuity and contact resistance across bonded bump arrays. This links surface valence-state control directly to bonding yield, mechanical integrity, and electrical performance in advanced packaging. Figure 1. OM of hybrid bump (a)before and (b)after VUV/citric acid treatment Figure 2. Mechanism of passivation layer formation on Cu surface RESULT AND DISCUSSION VUV treatment acted primarily as an organic-removal and surface-activation step. After 20 min VUV exposure, the C:Cu ratio decreased from 2.9 to 0.09 and the water contact angle decreased from 76.3 deg to approximately 30.6 deg, indicating effective removal of adventitious carbon and improved wettability. Cu 2p and Cu LMM spectra after citric acid treatment showed suppression of Cu2+-rich hydroxide-related components, while the near-surface region remained dominated by Cu0+/Cu1+-related states. Figure 3. XPS C1s spectra of VUV exposed copper surface Figure 4. (a)XPS Cu2p spectra & (b)Cu LMM Auger spectra of VUV + citric acid treated copper surface Citric acid served as the oxide-state control and passivation step. The 5 wt.% condition provided an effective balance between Cu oxide removal and surface stability. After sequential 20 min VUV + 5 wt.% citric acid treatment, XPS indicated a Cu0/Cu1+-dominant surface with strong suppression of Cu2+ species and residual C–O/O–C=O signals related to Cu–citrate/carboxylate termination. This citrate-derived layer stabilizes Cu valence states, suppresses localized re-oxidation, and supports low-temperature Cu–Cu bonding compatibility. Figure 5. Contact angle of VUV treated copper surface Figure 6. AFM morphology measurement on copper surface, (a) No VUV, Image Ra = 3.9 nm, (b)20 min VUV, Image Ra = 2.5 nm Figure 7. Cross sectional image of the bonded interface CONCLUSION Sequential VUV–citric acid passivation demonstrated improved Cu bump oxide-state control, queue-time stability, and bonding compatibility in Cu–Cu hybrid bonding structures. Initial low temperature bonding trials are promising, and further roughness control, electrical reliability evaluation and contact resistance studies are going on.
|
|
Low Thermal Budget Hybrid Bonding for Fine Pitch 3D IC Integration with High Interfacial Reliability using Fine-grained Copper
發表編號:S14-6時間:14:15 - 14:30 |
![]()
Paper ID:TW0055 Speaker: Jia-Juen Ong Author List: Jia-Juen Ong and Chih Chen
Bio: Jia-Juen Ong received his Ph.D. degree in Materials Science and Engineering from National Yang Ming Chiao Tung University (NYCU), Taiwan, in 2023. He is currently a Postdoctoral Researcher at NYCU. His research focuses on low-temperature Cu–Cu direct bonding, Cu/SiO₂ hybrid bonding, and heterogeneous integration technologies for advanced packaging applications. He has authored and co-authored more than 30 journal and conference publications in the fields of copper bonding and advanced packaging.
Abstract: As the desperate demand of high-performance computing (HPC) driven by artificial intelligence (Al) applications such as next-generation high-bandwidth memory (HBM) toward beyond 16-Hi stacks or the hybrid integration with photonic (PIC) and electronic integrated circuits (EIC) in co-packaged optics (CPO). Heterogeneous integration with advanced 2.5D/3D architectures requiring Cu/SiO2 hybrid bonding with ultra-fine pitch and low thermal budget processes has become a crucial technology with urgent needs. Such low-temperature(<250 °C) processing prevents temperature-sensitive devices from damage and suppresses warpage of thinned stacked wafers and ensures high-precision alignment. In this study, we propose fine-grained Cu (FC-Cu) as bonding interconnects. Recently, FC-Cu has been recognized as another promising materials in Cu direct bonding due to the high density of grain boundaries, which serve as fast diffusion pathways and promote interfacial atomic diffusion, recrystallization, and grain growth across the bonding interface. Thus, demonstrating advantages for low temperature bonding process and aggressive interconnect downscaling in advanced packages. In this work, FC-Cu is deposited by tailoring the microstructure of the Cu using different plating parameters. Dense FC-Cu with grain sizes of 100~200 nm detected by a electron backscatter diffraction (EBSD) analysis and results shown a high-angle grain boundary fraction exceeding 90% are uniformly electroplated into Cu/SiO2 damascene structures with a diameter of 2 µm. During chemical mechanical planarization (CMP), dishing of the FC-Cu pads can be controlled to less than 3 nm enabling the SiO2 dielectric layers to contact first and form a Van Der Waals bond in the pre-bond stage. This subsequently drives micro-protrusion by the thermal expansion of the Cu pads during post-annealing process at 200 °C under vacuum ambient, yielding void-free Cu-Cu and SiO2-SiO2 bonding. The bonding quality is further analyzed by FIB-SEM and revealing well bonded interface with no obvious cracks and low interfacial void area fraction providing evidence of atomic diffusion bonding. Bonding strength further quantified by using die-shear testing, demonstrating adequate mechanical strength. In summary, low thermal budgets bonding process is compatible with back-end-of-line (BEOL) processes and reduces warpage in wafer stacks guaranteeing alignment accuracy. Through synergistic morphology control across the fabrication process, the FG-Cu unifies mechanical integrity and electrical performance under low thermal budget. This provides a highly reliable and cost-effective hybrid bonding pathway for ultra-fine pitch 3D-stacked devices such as HBM, CPO optical engines, MEMS, and other advanced packaging applications.
|
|
Direct Current Density Control of (111) Nanotwinned Cu in Additive-Free Electrolyte for Low-Temperature Cu-Cu Bonding
發表編號:S14-7時間:14:30 - 14:45 |
![]()
Paper ID:AS0107 Speaker: Jinmyeong Seo Author List: Jinmyeong Seo, Haneul Han, Byungkwan Kwak, SangHwa Yoon, and Bongyoung Yoo
Bio: Jinmyeong Seo is currently a Postdoctoral Researcher at the Advanced Packaging Center within the Hanyang Institute of Environmental and Energy Technology, Republic of Korea. He received his Ph.D. from Hanyang University, specializing in the electrochemical synthesis of advanced nanomaterials. His primary research focuses on next-generation low-temperature bonding technologies for advanced semiconductor packaging architectures, specifically targeting sub-100 degrees C and room-temperature bonding processes. His expertise includes Cu crystallographic texturing, precise microstructural manipulation, current-assisted bonding kinetics, and stress-induced bonding mechanisms. Through these innovative approaches, he conducts dedicated research to overcome the thermal and mechanical limitations of conventional interconnects in high-density packaging systems.
Abstract: ABSTRACT In three-dimensional integrated circuits (3D ICs), low-temperature Cu-Cu direct bonding is essential to prevent thermal stress. Crucially, this study validates the low-temperature bonding capability of highly (111)-oriented nanotwinned Cu (nt-Cu) fabricated completely under organic additive-free and continuous direct current (DC) conditions, thereby avoiding the complexities of conventional pulse electrodeposition. Based on a stress-relaxation mechanism where controlling the current density from 0.1 to 0.4 A/cm2 tailors the nanotwin fraction up to 50%, this work successfully applies these tailored microstructures to advanced packaging interconnects. Cu-Cu direct bonding at 240°C for 1 hour realized a completely defect- and void-free bonded interface. Furthermore, the complete absence of organic impurities eliminated boundary pinning sites, enabling the observation of active, micrometer-scale grain growth directly across the bonded interface, which optimizes both mechanical and electrical properties for next-generation advanced packaging.
INTRODUCTION Next-generation 3D ICs require reliable, low-temperature metal bonding to prevent thermal degradation and minimize residual stress. [1] Cu-Cu direct bonding using (111)-oriented nanotwinned Cu (nt-Cu) is highly advantageous due to its superior electrical and mechanical properties [2], alongside the high surface diffusivity of the (111) plane [1]. Conventionally, nt-Cu synthesis relies on organic additives or complex pulse electrodeposition. However, additives cause impurity incorporation at grain boundaries [3], while pulse plating increases industrial manufacturing costs and reduces overall production efficiency. To resolve these technical limitations, an additive-free direct current (DC) electrodeposition method is introduced, utilizing current density control (0.1-0.4 A/cm2) under low-temperature conditions to induce highly pure nt-Cu structures driven by a stress-relaxation mechanism. [4] Building upon this foundation, this work extensively validates the low-temperature Cu-Cu bonding capability of these additive-free films. By eliminating impurities, boundary pinning sites are removed, enabling the unique observation of active micrometer-scale grain growth across the joint interface at 240°C.
EXPERIMENTAL Cu films were electrodeposited using an additive-free 1.0 M CuSO4-5H2O electrolyte adjusted to pH 0.8 with sulfuric acid. The process was conducted at 0°C to restrict adatom surface diffusion and promote stress-relaxation-induced twin formation. The DC density was varied to tailor the microstructural transition. For bonding evaluation, 0.3 A/cm2 samples were utilized. Thermal compression was performed under a nitrogen (N2) atmosphere at 240°C and 2 MPa for 1 hour. Cross-sectional microstructures and the bonded interface were comprehensively analyzed via focused ion beam (FIB) microscopy.
RESULTS AND DISCUSSION Under low-temperature, additive-free conditions, the microstructure transitioned from nanocrystalline to (111)-oriented nt-Cu solely through DC density control. As the current density increased from 0.1 to 0.4 A/cm2, the nanotwin column density systematically elevated from 0% to approximately 50%. Chronovoltammetry and stress analyses revealed that a higher current density restricts the time available for adatom surface diffusion relative to charge transport, inducing high initial residual stress in the growing film. [4] To alleviate this elevated strain energy, (111)-oriented nanotwins are preferentially formed as a stress relaxation mechanism, which subsequently leads to a significant reduction in intrinsic macro-stress. This behavior aligns with the Strain Energy Release Maximization (SERM) model, where stress relaxation drives preferential crystallographic evolution. [4]
Thermal compression of the nt-Cu film electrodeposited at 0.3 A/cm2 demonstrated an exceptionally stable and defect-free joint interface at 240°C for 1 hour. Notably, active grain growth spanning several micrometers occurred directly across the original bonding interface. This phenomenon strongly deviates from conventional nt-Cu bonding literature, where interdiffusion is typically restricted to surface creep along the (111) planes without massive grain boundaries migration. [1] In this work, the use of an additive-free electrolyte successfully prevented the incorporation of organic impurities or co-deposited codeposits within the Cu matrix. The complete absence of these embedded impurities eliminated the grain boundary pinning sites (Zener pinning effect). [3] Consequently, the substantial stored strain energy and twin boundary defects within the nt-Cu acted as a powerful driving force, accelerating massive grain growth across the contact boundary during annealing. This distinct microstructural evolution effectively eradicates interfacial voids, minimizes electrical resistivity, and significantly enhances mechanical bond strength.
CONCLUSION In conclusion, this study successfully demonstrates a reliable low-temperature Cu-Cu direct bonding pathway utilizing highly pure, (111)-oriented nt-Cu films controlled solely via an additive-free DC electrodeposition process. By precisely optimizing the direct current density, the intrinsic stress-relaxation mechanism successfully tailored the nanotwin fraction up to 50% without requiring conventional organic additives or complex pulse current parameters. Thermal compression bonding of these tailored films at a reduced temperature of 240°C for 1 hour realized a completely defect- and void-free bonded interface. Crucially, the complete absence of organic impurities eliminated boundary pinning sites, enabling the unique observation of active, micrometer-scale interfacial grain growth, which provides a highly dependable integration solution for next-generation 3D packaging applications.
|
|
A Novel Double-Layer Copper Architecture for Enhanced Storage Stability and Low-Temperature Cu-Cu Direct Bonding
發表編號:S14-8時間:14:45 - 15:00 |
![]()
Paper ID:TW0075 Speaker: Ke-Wei Hsieh Author List: Ke-Wei Hsieh, Chih Chen
Bio: Ke-Wei Hsieh is currently a Ph.D. student in the Department of Materials Science and Engineering at National Yang Ming Chiao Tung University (NYCU), working under the supervision of Professor Chih Chen. His research primarily focuses on Cu-Cu direct bonding, low-temperature bonding for 3D IC applications, and advanced packaging technologies.
Abstract: The downscaling of semiconductor devices has positioned advanced packaging at the forefront of microelectronics evolution. Cu-Cu hybrid bonding is indispensable for achieving ultra-high input/output (I/O) densities, circumventing traditional solder joint limitations. However, conventional thermo-compression bonding requires processing temperatures exceeding 300°C, imposing severe thermal budgets. Consequently, engineering robust Cu interconnects for low-temperature bonding is imperative. Nanocrystalline Cu (NC-Cu) enables low-temperature bonding due to its massive internal energy and dense grain boundaries serving as rapid atomic diffusion paths. However, NC-Cu is highly susceptible to room-temperature self-annealing, dissipating its thermodynamic driving force. Here, we investigated the microstructural evolution of electrodeposited Cu films—prepared with Chemleader Corporation additives—across different current densities. Analysis revealed highly current-dependent grain sizes: 1 ASD yielded coarse grains (~600 nm), 4 ASD showed intermediate grains (~200 nm), and 12 ASD produced NC-Cu grains (~80 nm). After one month of room-temperature storage, the 1 ASD and 4 ASD samples maintained structural integrity, whereas the 12 ASD sample underwent severe self-annealing, abnormally coarsening to over 3 μm. To clarify this disparate stability, Secondary Ion Mass Spectrometry (SIMS) was conducted. Results showed an inverse correlation between current density and impurity incorporation. The stable 1 ASD film trapped higher impurity concentrations (C, N, O, S, Cl), effectively pinning grain boundaries. Conversely, the 12 ASD layer contained far fewer impurities, leaving its active grain boundaries unpinned and thermodynamically unstable. Bonding tests were conducted at 200°C for 1 hour. Due to insufficient diffusion, the 1 ASD sample exhibited prominent interfacial gaps, and the 4 ASD sample retained a distinct straight bonding interface. Although the freshly prepared 12 ASD sample demonstrated remarkable cross-interface grain growth, its susceptibility to self-annealing severely limits the practical storage window, creating a critical material trade-off. To overcome this limitation, a double-layer Cu architecture was engineered via a single-bath electrodeposition process. A coarse-grained foundation was formed at 1 ASD, followed by switching current density to deposit a thin (<1 μm) NC-Cu layer on top. Because this top layer is thin, it lacks sufficient energy to initiate self-annealing. Evaluations confirmed the as-deposited top NC-Cu grains were ~80 nm. Even after one month of storage, the cross-sectional structure remained stable, and the top NC-Cu grain size stayed below 100 nm, preserving its bonding energy. Leveraging this stabilized driving force, bonding was successfully achieved at 200°C. The double-layer structure exhibited a dense, zig-zag bonding interface. Transmission electron microscopy (TEM) validated that curvature-driven thermodynamic imbalance caused the foundation's coarse grains to consume the top NC-Cu grains. This cross-interface grain growth successfully eliminated interfacial defects, providing a promising and reliable solution for next-generation advanced packaging.
|
|
|